Dear friend

Generally mechanical tests prepared from a radiography accepted test assembly which is welded in predefined conditions. Such tests are tensile (all weld meta), impact and in few cases transverse tensile, hardness and bend test. Also chemical analysis from weld metal or rod may be added. (for details you have to refer to the related std.)

About the quality, all approved producers shall satisfy minimum requirements indicated by standards. But the subject is how much they can be overqualified. They work on the usability of they products and improving the consuming time and economical issues. So the producer is very important and some specifications require re-qualification in case of changing welding consumables producers.

Regards


On Wed, Oct 30, 2013 at 4:20 PM, Kumar kerala <sk7920541@gmail.com> wrote:
Dear All,

Please share with me what all are the common tests(mechanical and
other) done for the testing of  elecetrodes & filler wires to check
their integrity ? also the changes of country of origins play
importatnt role on quality ?

thanks in advance,
Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...