[MW:19067] RE: 19048] Mode of Metal transfer for GMAW

Dear Pradip,

   There are 4 modes of metal transfer available for GMAW process.

1.       Short circuit

2.       Globular

3.       Spray( For Argon use)

4.       Pulsed

 

In your case short circuiting mode will be given better result than compare with other modes of transfer, but make sure that your welder skill is playing major role to maintain torch angle etc..

 

Regards,

J.V.S.Hemanth kumar

 

Senior Engineer

Operations I Welspun Middle East Pipes LLC

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pradip Ghosh
Sent: Wednesday, October 23, 2013 7:39 AM
To: materials-welding@googlegroups.com
Subject: [MW:19048] Mode of Metal transfer for GMAW

 

Dear Expert,

 

Can any one tell me that what are the metal transfer mode available for GMAW and what type of metal transfer is suitable for down hand bottom fillet welding in MAG/GMAW

 

 

Pradip Ghosh

 

QA/QC Engineer

 

Mott Mac Donald 

 

 

 

 

 

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...