Re: [MW:19141] API 1104

You need to qualify a repair welding procedure

From: Ghaith NDE <ghaithnde@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; John Henning <jhenning@deltak.com>
Sent: Wednesday, October 30, 2013 6:35 PM
Subject: [MW:19127] API 1104

Dear
I use on site as welding process  is GMAW automatic machine as 1104 and so my  qestion can I repair the defects if it discovered during RT by using SMAW manual and for knowlage smaw as wps and PQR are qualified   .
regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...