Monday, October 28, 2013

[MW:19088] ASME Sect IX-Qualifying PQR for ASTM A333 Grade 8

Dear Experts

Pls share your expertise in qualifying PQR
 
ASTM A333 Grade 8 ( UNS K81340 ),

CVN at -195 deg celcius.

P.No- 11A/ Group No - 1.

Min Dia 2" / Max Dia 8".

Min Thk-11.0mm / Max Thk - 32.0mm.




 2" and below - 100% GTAW.


Above 2 " - Intend to Weld Process - GTAW + SMAW , GTAW + FCAW.

Must comply to NACE MR0175.

Advise suitable welding consumable from  ESAB / Lincoln/Sanvik..etc

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...