[MW:19097] cracks in acroalloy tooth during welding

Dear Experts,
Acroalloy (C-.22-.27, Cr 1.5, Mo 1, Ni 3.5%) And hardness 340-460 BHN.
electrode used-E71T1 with CO2 shielding
Preheat 300 degree C
interpass temp. 175 degree c.
During welding of above acroalloy tooth with mild steel shell a crack was found on the surface of tooth even using proper preheating parameter. we didn't use proper PWHT for the joint. in some of the tooth a longitudinal crack was observed. kindly suggest me the reason for the crack. Is it PWHT or something else.

Regards
Raj Gupta
L&T

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...