FIRST MY CASE WITHOUT IMPACT TEST REQUIREMENT
IF I HAVE PQR for P-No. 1 Gr.No.1 to P-No. 1 Gr.No.1
I CAN USE IT TO WELD P-No. 1 Gr.No.1 to P-No. 1 Gr.No.2 ,THAT IS
THE MEANING OF SUPPLEMENTARY ESSENTIAL
EZZAT
---------- Forwarded message ----------
From: george.dilintas@gr.bureauveritas.com
Date: Tue, 29 Oct 2013 11:53:41 +0200
Subject: Re: [MW:19112] Change in Supplementary Essential Need re-qualification?
To: materials-welding@googlegroups.com
It needs
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
Prelude FLNG ASME Subject Matter Expert
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Korea cell phone: +82 10 2777 8922
From: Ezat Adel <ezatadel2008@gmail.com>
To: materials-welding@googlegroups.com
Date: 29/10/2013 11:25
Subject: Re: [MW:19109] Change in Supplementary Essential Need
re-qualification?
Sent by: materials-welding@googlegroups.com
dear Dr. Georgios Dilintas i need your confirm it is need requalification
or did not need.
On Oct 29, 2013 11:05 AM, <george.dilintas@gr.bureauveritas.com> wrote:
Yes it does
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
Prelude FLNG ASME Subject Matter Expert
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Korea cell phone: +82 10 2777 8922
Inactive hide details for Ezat Adel ---29/10/2013 10:57:21---Dear
Experts, i need your clarify that the changes in material groEzat
Adel ---29/10/2013 10:57:21---Dear Experts, i need your clarify that
the changes in material group number with the
From: Ezat Adel <ezatadel2008@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Date: 29/10/2013 10:57
Subject: [MW:19105] Change in Supplementary Essential Need
re-qualification?
Sent by: materials-welding@googlegroups.com
Dear Experts,
i need your clarify that the changes in material group number with
the
same p number need another welding qualification or not.
my case i have WPS for A312 grade TP 316, P no. 8 , group no. 1 to
itself.
it's right to use it to weld A312 grade TP 310s, P no. 8 , group
no.
2 to itself.
Ezzat
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding
+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel
views and meant for educational purposes only, Users must take their
own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google
Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it,
send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
This message contains confidential information. To know more, please
click on the following link: http://disclaimer.bureauveritas.com
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding
+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel
views and meant for educational purposes only, Users must take their
own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google
Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it,
send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding
+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an
email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
This message contains confidential information. To know more, please
click on the following link: http://disclaimer.bureauveritas.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google
Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send
an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment