Sunday, September 1, 2013

Re: [MW:18560] Re: How to select the IQI wire

Dear Mr. Raheel/ Venkat,

If no project spec. is applicable, selection of IQI shall be as per Table T-276 of Article 2 of ASME Sec. V. For material selection group please refer SE-747 of ASME Sec. V.

Thanks & regards,


C. R. GANDHI          


From: Raheel Arif <raheel.qc@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, August 31, 2013 12:25 PM
Subject: [MW:18547] Re: How to select the IQI wire

Dear All,

Let me know what is the difference between ASTM, FE EN & DIN wire. What material is suitable for which wire?

Regards,
Raheel Arif

   

On Monday, August 2, 2010 8:48:53 AM UTC+4, venkat ramana wrote:
Dear All,
 
let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.
 
Thanks & Regards
venkat (QC)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...