Dear Experts,
I have a query on MR-0175/ISO 15156 and the and the applicability of <22 HRC restriction on 13% Chromium components and overlay.
The following info is regarding a Valve:
· Other wetted components (such as stem, Bonnet bush) made of forging and bar are double tempered to bring the hardness under 22 HRC.
· The obturator material is ASTM A 216 Gr. WCB and the Overlay is 13% Chromium (1.6 mm thickness).
· However, for the 13% Chromium overlay to be brought under 22 HRC, double tempering would take the base material WCB to >720°C, at which the base material properties would be affected at the cost of bringing the overlay hardness under 22 HRC
How is the Hardness issue of 13% chromium overlays addressed in the industry?
Thank you for taking time to reply.
Regards
Ram
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments