Dear Anban ,

You can refer from the terminology section AWS A3.0 and other welding technology books for the following in more details :

1) Autogenous Weld -      A fusion weld made without filler metal.  - Examples are Solid Phase welding, resistance welding , sometimes GTAW used in tube to tubesheet in Heat Exchangers without adding Filler .
2) Homogeneous Weld -   A fusion weld made with filler , in which the filler is similar to basemetal chemical and mechanical properties . Examples, Arc welding like SMAW, GTAW, FCAW, SAW, GMAW etc.
3) Heterogeneous Weld -  A fusion weld made with filler material which is different from the parent material - Examples are Soldering and Brazing .

Hope this clarifies .

Cheers,
Saravanan ,
Korea


On Mon, Sep 23, 2013 at 11:28 AM, Anban <gane2478@hotmail.sg> wrote:
 Dear Experts
 Pls define with some samples and its applicability
 Thanks
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...