1- During PQR Testing.. you have to consider actual thickness of the Test Specimen, not of the MTC.
2- Practically Impact test can be possible for specimen  >2.5 MM thk after Machining. In your Case-2 , I suggest you to go-through your project spec once again for exact requirement.

Regards
Anil Kumar


On Fri, Sep 27, 2013 at 10:20 PM, Ahmed Husain <ahmraha@yahoo.com> wrote:
Dear All,
 
I have following two question related to qualification of WPS and PQR  with impact testing.
1. As per ASME IX para 403.6: where T is less than 14 in.(6 mm), the minimum thickness qualified is 12T.
my question is, if i have a material MTC stating thickness 6.4 mm, can i refer as 1/4" in PQR/WPS to get the benefit of 1/2 T qualification range.
2. As per project specification, if heat input range varies considerably in different passes, then additional impact test is required from different passes. If a test piece thickness is 6.4 mm, is it practical to take impact test specimen from different passes.
 
Your valuable reply will be highly appreciated.
 
With best regards,
Ahmed H.
ABSG Consulting, KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...