Re: [MW:18816] Post heating required for alloy steels after welding

 Preheat & Post heating  are mandatory for low Alloy steels... Cr-Moly steels are very brittle in nature and there is high chance of brittle fracture if you perform welding directly.

So, First you have to do pre-heat to make the Bevel end area and HAZ area soften. and then perform the welding by maintaining the pre-heat temperature ...once welding is completed, you should immediately do post heating  and cover the weld joint with fire blanket ....so that the grain structure & material properties wont effect and to avoid delay cracking.


Qualify a test coupon for better analysis .


regards
Anil




On Mon, Sep 30, 2013 at 8:12 AM, PK M <pkmqaqc@gmail.com> wrote:
Dear Experts,

Why post heating required for alloy steels after welding? I want to know that what is the procedure and acceptance of Post heating of alloy steel in piping specification like Section 31.3, 31.1 or Section VIII, API recommendation practices ?

 Thanks,

Pkm

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...