Re: [MW:18552] Need supplier address for induction heating

You can order one with
Magnallenz
B/4 Sakariba Esatate, G.I.D.C. Phase – IV,
Vatva, Ahmedabad – 382445
Gujarat (INDIA)
Phone No.: +91-79-25840023 / 25840024 Fax : +91 – 79 – 25841065
E-Mail : contact@magnalenz.com , magnalenz@gmail.com

Reg,
K.Saravanan


On Sat, Aug 31, 2013 at 3:00 PM, Sankaran Sp <subasankaran@yahoo.co.in> wrote:
Dear experts,

I need one help from you,We are in need to pre- heat the valve body by induction heating method before production welding. Do you have any supplier in india & abroad ? to design & supply the induction pre heating system (System consists of power source,water cooled  flexible coil, thermo-couple with digital thermo meter and necessary items) for our application.
Our valve body material will be : ASTM A 216-WCB,A217-WC6,WC9 & C12A
Pre heating temperture will be 100,150,200DegC
Kindly do the needful to proceed further.

Regards,
sankaran.Sp
welding & metallurgy expert

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...