Dear Kunal,
There is no specific code or standard requirement of ‘lux’ for RT interpretation. Lux requirement is for Visual, MPI &LPI.
RT film viewer must have variable light intensity adjustment and able to read the maximum permissible density, which is in general 4.0.
Thanks,
With kind regards,
M. Vedaraju
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sonu Shahu
Sent: Monday, August 19, 2013 5:29 AM
To: materials-welding@googlegroups.com
Subject: [MW:18470] LUX FOR INDUSTRIAL RADIOGRAPHY FILM INTERPRETATION
Dear Experts,
How much lux for film interpretation by film viewer?
what is reference code & specification for this?
THANKS & REGARDS
SONU M SHAHU
--
kunal
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments