[MW:18480] Scope of connecting weld of two pressure vessels Interpretation to U-1(e)(1) of ASME Sec VIII div 1

Two pressure vessels, each with a separate U symbol and Manufacturer's Data Report, are welded together at their respective nozzles. It is not within the scope of Sec VIII div1 as per U-1(e)(1)(a). Then what requirements (PWHT/NDE/Hydro etc.) and certification to be followed at site? below interpretation states the requirements are those indicated by the jurisdictional authorities at the point of installation.


Interpretation: VIII-78-136

Subject: Section VIII, Division 1, Scope

Date Issued: October 27, 1978

File: BC78-580

Question: Two pressure vessels, each with a separate U symbol and Manufacturer's Data Report, are welded together at their respective nozzles. Is the weld itself subject to the requirements of Section VIII, Division 1?

 

Reply: No. U-1(e)(1)(a) indicates that the geometry of pressure-containing parts includes the welding end connection for the first circumferential joint for welded connections. Further, this welding is being done subsequent to the stamping of the vessel. The applicable requirements are those indicated by the jurisdictional authorities at the point of installation.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...