Re: [MW:18463] Welder qualification for weld repair

Dear Swapnil,

In cross country pipeline project,we are using Downhill welding  for mainline welding.But in case of repair we are using we using Root -Uphill & Other passes downhill welding.

As per API 1104 Direction of welding is a essential variable.

So it is necessary to qualification separately.


On Wed, Aug 14, 2013 at 5:06 PM, swapnil sonavane <sonavane.swapnil@gmail.com> wrote:
Dear Experts,

Hello,

I am having WPS qualified for repair procedure according to API 1104.

Is it mandatory to qualify the welders separately for repair welds?

Any reference from specification is available for this?

--
Best Regards,

Swapnil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--

Thanks & Regards,  

?

Joydev Dalai

Sr.Engineer  (QA/QC)

+91 7894454980
Fernas Construction India PVT.Ltd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...