Re: [MW:18539] Re: major difference of B7& B7M

Dear rahul,
I understand that normally b7m bolts are preferred in corrosive environments.. can u pls elaborate the difference on the account of corrosion resistance.I.e. why b7m has better corrosion resistance. .
Thanks in advance;

Regards,
Nishant Nair

Sent from Yahoo! Mail on Android



From: Rahul Singh <rahul1127@gmail.com>;
To: <materials-welding@googlegroups.com>;
Subject: [MW:18535] Re: major difference of B7& B7M
Sent: Wed, Aug 28, 2013 11:09:19 AM

Dear Ali,

Your specification calls the requirement for B7M to avoid the corrosion under insulation. B7M bolting is often opted for in corrosive environments due to its heat treatment & hardness.

B7  bolting also can be used if it is used for non exposed to corrosive environment which means we can substitute the B7 bolting with B7M for corrosive environment.

Regards

On Tuesday, August 27, 2013 1:24:18 PM UTC+3, Ali Asghari wrote:
Dear All
What are differences between B7,B7M ?(except as torque value,yield strength)
In our specification usage of B7M confined under insulation.why?
When we can B7 replaced by B7M with regard to service condition?or is it possible with regard to dissimilar strength ?
Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...