Hi Siva,

Please review the attached PDSs MIG & TIG Brazing filler alloys . As you need assistance for your project work hence this mail. For more details on dissimilar brazing you may visit Fontargen web-site thru the link below my signature. We can discuss more on our products  out of forum’s domain .

 

Hope this helps..

Thanks

 

With Kind Regards

 

Amitabha Bhattacharya

Head-Application Technology

 

Bohler Welding Group India Pvt. Ltd.

A-140, Road No 23, Wagle Industrial Estate

Metropolitan, Ground Floor

Thane  400 604, India

Ph: +91 22 2582 8855/4228 4400

Mobile ;+91 9833998246

 

Email: amitabha.bhattacharya@bwgindia.com

Web: www.bohlerweldinggroupindia.com

A Böhler Welding Group Company

 

This email message and any attachments are for the sole use of the intended recipient(s) and contain confidential and/or privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message and any attachments

 

 

 

 


From: Siva Chidambaram <mechsivachidambaram@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 15 August 2013 3:07 PM
Subject: [MW:18437] Bronze to carbon steel welding.

 

Hi Friends,

 

In my project, there is welding between bronze and carbon steel. Can anyone kindly say me what electrode to be used for welding.

 

M. Sivachidambaram

+971561530899

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...