Thursday, March 31, 2011

RE: [MW:10542] Welder Qualification

Yes, as per ASME SEC IX - EDITION 2010  QW-190 , you can also qualify a welder by UT instead of RT.

Regards,

 

Di Prinzio, Juan Carlos

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de K U Masood Ahmad
Enviado el: miércoles, 30 de marzo de 2011 12:18
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:10533] Welder Qualification

 

No you cant

 

On 30 March 2011 18:28, Ramesh Barot <rameshnbarot@yahoo.com> wrote:

Dear all experts,

 

Can we qualify welder by UT?


 

Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
K U Masood Ahmad

Industrial Services
SGS India Private Limited
Himachal Sorang H.E.P.
GSM +91 - 9805997411

www.sgs.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Información de ESET Smart Security, versión de la base de firmas de virus 6002 (20110331) __________

 

ESET Smart Security ha comprobado este mensaje.

 

http://www.eset.com



__________ Información de ESET Smart Security, versión de la base de firmas de virus 6002 (20110331) __________

ESET Smart Security ha comprobado este mensaje.

http://www.eset.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...