I think,this is not a backing,because this is to make sure for the welder confirmation. it is happen in normal practice that after welding of single v groove of plate and to be confirmed by visual to confirm the full penetration..and if the penetration is good...many(All) times the welder need to confirm by themself by grind to some depth after confirm by visual (1 or 2mm max..) to make it look good appearnce as well as to avoid any discrepancies in RT.(even it can accept in Rt without grinding)
 
As far as my experience and Customer,AI witness.. it was accepted as without backing...

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 3/23/11, John Henning <jhenning@deltak.com> wrote:

From: John Henning <jhenning@deltak.com>
Subject: [MW:10464] RE: 10463] Backing
To: materials-welding@googlegroups.com
Date: Wednesday, March 23, 2011, 9:41 PM

YES – it is welding with backing.

 

See QW-402.4, non-essential variable for both SMAW and GMAW and an essential variable for welder performance qualification for both processes per QW-416.

 

"QW-402.4  The deletion or the backing in single  welded groove welds.  Double welded groove welds are considered welding with backing."

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Venkateswaran
Sent: Wednesday, March 23, 2011 4:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:10463] Backing

 

 

As per ASME SEC IX ,we qualified PQR(SMAW/GMAW process) with 8mm/10 mm thickness plate full penetration welding( Root Land:1mm to 1.5 mm) as root ,hot and cap welding and then back/root side of plate was grounded(approx 2mm) to sound metal and one pass of cap welding was done in root side.

My question is whether is method is considered as welding with backing or with out backing it is considered as backing. how?

 

 

 

Regards,

 

kvr

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...