[MW:10518] Re: SS 304 WIRE WELDING

Hi
Can you please tell wht is the length of the wire for welding.
One method is to weld by flash welding and also you can use micro TIG
welding (welding with a very Low weld parameters) with proper
fixturing.
But its better if you can provide the dimension of material to be
weld.

Regards
Sandeep Kumar


On Mar 27, 3:49 pm, com...@rediffmail.com wrote:
> Dear Friends,
> We are looking for the solution to weld 3 mm SS 304 wire.  the tolerances are as follows
> Weld Point Material formation and demormation +/- 0.15 mm
> Could you please provide us the best solution to control this in production.
> We have the daily production target of 100000 pcs.
> Warm Regards,
> KUNAL KHATRI

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...