ِِAccording to ASME IX you have two options
1- By RT
2- By DT
No other option is permitted

From: Ramesh Barot <rameshnbarot@yahoo.com>
To: Materials Welding <materials-welding@googlegroups.com>
Sent: Wed, March 30, 2011 2:58:06 PM
Subject: [MW:10529] Welder Qualification

Dear all experts,
 
Can we qualify welder by UT?

 
Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...