[MW:10527] Clubbing of PQRs in AWS D1.1

Dear All

Can I club 3 PQRs to make a WPS as per AWS D1.1

I have 1 PQR with SMAW in 6GR position, 1 PQR with FCAW in 6GR position and a 3rd PQR with SMAW + FCAW in 6G position. My requirement is to make a WPS with combination process of SMAW + FCAW in 6GR position.

And for combination of PQRs what all parameters can be referred in the WPS?

Please give your comments.

Thanks and Regards
Harikrishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...