HI
There are a no. of european standars for materials grade.
Tell which material you arelooking for, so that I can tell you the
relevant standard.

Regards
Sandeep Kumar

On Mar 29, 12:27 am, john clough <johnclough...@hotmail.com> wrote:
> Dear Sirs
> I need to review material certificates regarding material grades, mechanical tests etc, these material certificates are ISO 3-1, I am familiar with ASME Section 1X which is where I would look for this information if I was working to ASME Standards, where would I find the same information working to ISO standards.
>
> Thankfully
>
> John                                      

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...