Saturday, March 26, 2011

[MW:10491] AFTER STRESS RELIEVING

Dear Experts,
 
One joint we found some base metal defects[A sort cluster pore]which is slightly away from the weld metal.can we grind and check.please suggest what kind of corrective action to be taken with valid reasons.Also please let me know "DOS & DONT'S AFTER PWHT".
With Best Regards
Sampath

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.