[MW:2038] RE: 2035] A number in case of Low alloy steel welding with E-7018 Electrode

Hi!

If the weld metal chemistry is not falling under "A" no specified .In this
case we can use that PQR/WPS for specific actual chemistry with THE BRAND
and THE ACTUAL CHEMISTRy for that type of base metal welding(In short it is
a Brand and base metal restriction)

Regards

Hegde P.B.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of JASPAL SINGH
Sent: Monday, April 27, 2009 1:03 PM
To: Materials & Welding
Subject: [MW:2035] A number in case of Low alloy steel welding with E-7018
Electrode


I did PQR of Low alloy steel with E-7018-I electrode.

As 'A' number is essential variable.

What should i write over there , because weld metal chemical
composition after dilution will not be A-1.

Regards

Jaspal Singh
9996624244

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...