Dear Sadique,
 
For welder qualification Minimum length of  6" (150 mm) required to be radiographed , and shall include entire weld circumference of pipe,it is same for all pipes, for small bore pipe , multiple coupons to be required but it should not exceed 4 coupons,
 
If you want more details refer QW-302.2  , QW-304 of ASME Section IX
 
Mubarak.

 
On 4/19/09, sadique sheikh <mails_sadique@yahoo.com> wrote:
Hi all of you.
For welder qualification what should be the minimum length of specimen required? Is it same for all sizes of pipes? Can i get the referance from section 9 for this?
Regards
Sadique

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...