Monday, April 20, 2009

[MW:1991] RE: cleaning of copper pipes

No idea about pipes. But the standard method for cleaning copper wire rod during wire drawing process is pickling in hot 20% sulfuric acid followed by rinsing in water.  

Any suggestions from members?


From: venu moturu [mailto:moturuvenu@yahoo.com]
Sent: Sunday, April 19, 2009 5:30 AM
To: Bathula Raghuram (Mumbai - PIPING); sanjay
Subject: cleaning of copper pipes

 

Dear Raghu,

 

Could you pl. advice/ suggest  me any procedure /  cleaning method  available  for  removing tarnish on copper  pipes ....

 

 

Regards

venu 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...