Yes,u can use. Both are P1 Gr. 1.
 
Mostly SA333 Gr. 6 will be used for low temperature. Confirm the impact test requirement if any. SA333 Gr. 6 may asked for impact test. Confirm the PQR is tested lower than the required MDMT.
 
Regards,
Muhammed Ibrahim

2009/4/22 parviz farhadi <parvizfarhadi@gmail.com>
Dear All,
 
Is it possible to use WPS of ASTM A106 Grade B and its PQR for ASTM A333 Gr 6?
 
Regards,
Parviz





--
Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...