Yes you can use 15mm wide strip ,There are firms can slit the strip to required size. 15mm width strip can use on 20mm base having less distortion with spirel welding.

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ravinder Sharma
Sent: Wednesday, April 29, 2009 5:46 PM
To: materials-welding@googlegroups.com
Subject: [MW:2061] 10mm wide Strip

 

 

Hi friends,

 

Have anybody tried 10mm X .05 mm strip for corrosion resistant cladding to avoid distortion of less volume  component?

Is it comparable to FCAW option?

Is there any source to get strip of this size?

 

Ravinder Sharma

ISGEC, Yamuna Nagar.

 


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...