Wednesday, February 25, 2009

[MW:1641] Re: flatolet

The flatolet is basically "olet" to be used on flat surface or on the very
large run sizes (where the difference of curvature becomes less and less
significant. As per bonney forge catalogue, the weldolet for run sizes
larger than 36" (DN 1800) will be considered as flatolet.

Please note that one needs to specify this in the purchase order whether
you require flatolet.

Hope to have clarified

Best regards,

Prasad


"Sreejith.Nair"
<fizzyshadow@gmai
l.com> To
Sent by: materials-welding@googlegroups.com
materials-welding cc
@googlegroups.com
Subject
[MW:1639] flatolet
25/02/09 06:42 PM


Please respond to
materials-welding
@googlegroups.com

can anybody please explain what a flatolet is?? it would be a great help if
a picture of the same can be posted.



Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...