Tuesday, February 17, 2009

[MW:1594] Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

Can anybody suggest the consumable brands/mfr name who can give guaranteed results (if possible pl. attach data sheet)  for high temperature Stress Rupture testing of all batches of welding consumables used at 1000°F & 30ksi stress. The time of failure shall exceed 900 hrs.

Thanks in adv.



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS