DEAR FRIENDS,

FOR SS304L TIG WELDING WHAT FILLER WIRE CAN USE AT 4.5K ( - 269
CENTIGRADE) TEMP.

ALSO FOR THIS WPS,PQR AT WHAT TEMP. I SHOULD DO IMPACT TEST & WHAT IS
THE ACCEPTABLE LIMIT FOR IMPACT TEST OR LETARAL EXPANSION TEST

PLS GIVE ME REPLY

THANKS & REGARDS,