[MW:1587] Re: weld profile

Dear Mr. Ali Asghari,

In general you should perform such Burr grinding treatment on all
highly stressed / loaded weld connections in a structure. The problem
is that most structures have a little bit different lay-out for the
branch connections therefore a FEM calulation should be performed
before you cand determine the welds which should be treated. In
general you can say that all connections of interest are in the top
side of such structures. I have only little expirience with branch
connections in Offshore structures and more in Bridges, there we not
treat the full circumferential weld length but only the highly loaded
side, I'm not sure if you can / may apply such on Offshore structures
as well.

Best Regards,


Herman Pieper

On 14 feb, 05:41, Ali Asghari <asghari...@rocketmail.com> wrote:
> Dear Mr Herman Pieper
> thanks for your completely response.
> can u guide me which T,K,Y joints in offshore jacket,must be grinded?
> thanks adv
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...