Monday, February 16, 2009

[MW:1591] Re: Nominal Thickness

Hi Babu,
               Nominal thickness means pipe schedule thickess.
Example pipe size 6" sch 40, A 106 Gr B , in this case sch 40 (7.11mm) is nominal thickness.
Actual thickness means measured thickness but this measured thk should be with in tolerance as per applicable code.
 
Louis
Toyo Engg - Singapore

--- On Sat, 14/2/09, babu k <kbabupsg@gmail.com> wrote:
From: babu k <kbabupsg@gmail.com>
Subject: [MW:1582] Nominal Thickness
To: materials-welding@googlegroups.com
Date: Saturday, 14 February, 2009, 9:49 PM