[MW:1619] FW: API 5L Gr B and A 106 Gr B


Dear ALL,

Please explain the difference as asked my Mick....., I am forwarding this mail to the group because I know this mail will reach to experts and they can reply in better way.

Thanks and regards,

Rafique


From: crc1199@hotmail.com
To: rafiquenaik@hotmail.com
Subject: API 5L Gr B and A 106 Gr B
Date: Tue, 24 Feb 2009 13:15:47 -0500

Dear Rafique,

Please explain me what is the difference between API 5L Gr B  and  ASTM  A 106  Gr.B  pipes.

Regards,

MICK


Access your email online and on the go with Windows Live Hotmail. Sign up today.

Akshay Kumar takes on the two reigning Bollywood Khans. Catch the action on MSN Entertainment! Check it out!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...