Monday, August 25, 2008

[MW:1061] Re: PWHT Furnace

Dear Chetan and other friends,

Gas fired furnace is cost effective compare to Electrical one.
Gas fired furnace can be made of bigger sizes to accomodate bigger size of components. Electrical furnace is suitable for smaller size only where test coupans or test pieces are to be heat treated.

Even In gas fired, Natural Gas is better than LPG but offcourse depends upon availability and necessary infrastructure. I am not aware about UAE condition as far as availability of NG and LPG.

hope I answered your query.

Regards,

Rajesh B. Patel
Abu Dhabi


--- On Mon, 8/25/08, Chetan Parekh <cpp1506@gmail.com> wrote:

> From: Chetan Parekh <cpp1506@gmail.com>
> Subject: [MW:1056] PWHT Furnace
> To: materials-welding@googlegroups.com
> Date: Monday, August 25, 2008, 2:00 AM
> Hi Friends,
>
> I need comparision between gas fired furncae and electrical
> induction
> heating furnace. Basically I am looking for advantage and
> disadvantage
> between these two heating media.
>
> Regards,
>
> Chetan Parekh
> Abu Dhabi
>
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...