Try using DCSP root, it should help you. Also, as Ramu has mentioned, please check the extent of magnetizm present
regards,
> Date: Thu, 31 Jul 2008 17:47:02 +0530
> From: orm24@yahoo.co.in
> Subject: [MW:986] Re: Root under cut
> To: materials-welding@googlegroups.com
>
>
> Dear Atul,
> If you are concerned more about to avoid root undercut, the only thing you need to do is to demagnetise the job near to wep and on wep with the help of demagnetising equipment and weld after demagnetising. You will get a smooth weld without any undercut.
> For one of our projects, we have over come the undercut problem by demagnetising and welding. This is for your information and for ferritic materials only.
>
> Regards
> Ramu
> +971-50-8249649-personal #
> +971-50-8181761-official #
>
>
> --- On Mon, 28/7/08, atul patil <atulpatil99@gmail.com> wrote:
>
> > From: atul patil <atulpatil99@gmail.com>
> > Subject: [MW:976] Re: Root under cut
> > To: materials-welding@googlegroups.com
> > Date: Monday, 28 July, 2008, 1:22 PM
> > to avoid root undercut
> > thanks in advance
> >
> >
> > On 7/27/08, Paresh Katvi <pkatvi@gmail.com> wrote:
> > >
> > > Dear Atul
> > >
> > > Ar you looking for information How to avoid root
> > undercut or NDT method to
> > > analisied under cut in most sensitive manner?
> > >
> > > please give further information.
> > >
> > > Regards
> > >
> > > Paresh Katvi
> > >
> > >
> > > On 7/22/08, atul patil <atulpatil99@gmail.com>
> > wrote:
> > >
> > >> Dear all
> > >> I am working with Gas export pieline in Kazakhstan
> > >> We are using 6010 electrode for root
> > >> & 8010 for fill cap
> > >>
> > >> we are facing the problem with root undercut
> > >>
> > >> Actually on the basis of radiography ( ISO 13847 )
> > doesnt ask to
> > >> cmpareason of density with parent metal It says
> > only about length
> > >>
> > >> Please guide
> > >> It is very difficult to prepare the calibration
> > block for UT ( Manual ) in
> > >> my city ( Atyrau )
> > >> Could you please guide
> > >> any suggestions welcome.
> > >> >>
> > >>
> >
> >
>
> Unlimited freedom, unlimited storage. Get it now, on http://help.yahoo.com/l/in/yahoo/mail/yahoomail/tools/tools-08.html/
>
> --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-