[MW:1005] Re: 1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503 -224 -GR. 28

OKAY. THANKS FOR YOUR INFORMATION.

REGARDS,

S.N.DAVE

--- On Thu, 8/7/08, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

> From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
> Subject: [MW:1004] RE: 1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503 -224 -GR. 28
> To: materials-welding@googlegroups.com
> Date: Thursday, August 7, 2008, 3:32 PM
> Why don't you check in EN 10222 for the required grade?
> As BS 1503 is
> obsolete, no use of searching for similar of equivalent
> grades.
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> shailesh dave
> Sent: Thursday, August 07, 2008 3:26 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE
> OF BS1503
> -224 -GR. 28
>
>
> YES IT IS FORGING MATERIAL.
>
> REGARDS,
>
> S.N.DAVE
>
>
> --- On Thu, 8/7/08, Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com> wrote:
>
> > From: Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com>
> > Subject: [MW:1000] RE: 999] Re: 993] EQUVIVALENT ASME
> GRADE OF BS1503
> -224 - GR. 28
> > To: materials-welding@googlegroups.com
> > Date: Thursday, August 7, 2008, 3:22 PM
> > Is it a forging material? BS1503 is superseded and
> replaced
> > by EN 10222,
> > please check?
> >
> > ________________________________
> >
> > From: materials-welding@googlegroups.com
> > [mailto:materials-welding@googlegroups.com] On Behalf
> Of
> > shailesh dave
> > Sent: Thursday, August 07, 2008 2:28 PM
> > To: materials-welding@googlegroups.com
> > Subject: [MW:999] Re: 993] EQUVIVALENT ASME GRADE OF
> BS1503
> > -224 - GR.
> > 28
> >
> >
> >
> > Dear Mr. Rohit,
> >
> >
> >
> > Thanks for the information. I have gone through it but
> it
> > does not say
> > specifically about224 - GR. 28
> >
> >
> > Would you pl. thorw some more light on this.
> >
> >
> >
> > Regards,
> >
> >
> >
> > S.N.Dave
> >
> > --- On Tue, 8/5/08, Rohit Bafna
> <rohit@tcreng.com>
> > wrote:
> >
> > From: Rohit Bafna <rohit@tcreng.com>
> > Subject: [MW:994] RE: 993] EQUVIVALENT ASME GRADE OF
> > BS1503 -224
> > - GR. 28
> > To: materials-welding@googlegroups.com
> > Date: Tuesday, August 5, 2008, 9:05 PM
> >
> > Dear Mr. Dave,
> >
> > Please look at
> http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm
> > <http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm>
> >
> > Regards,
> >
> > Rohit Bafna
> >
> > Director - Global Sales
> >
> >
> >
> > From: materials-welding@googlegroups.com
> > [mailto:materials-welding@googlegroups.com] On Behalf
> Of
> > shailesh dave
> > Sent: Tuesday, August 05, 2008 8:39 AM
> > To: materials-welding@googlegroups.com
> > Subject: [MW:993] EQUVIVALENT ASME GRADE OF BS1503
> -224 -
> > GR. 28
> >
> >
> >
> > DEAR MEMBERS,
> >
> > CAN ANYBODY LET ME KNOW THE EQUIVALENT ASME GRADE OF
> > BS1503 -224-GR.28.
> > WHERE FROM I CAN HAVE THIS INFORMATION AS READY
> RECKONER.
> >
> > REGARDS,
> >
> > SHAILEH
> >
> > QA/QC INCHARGE
> >
> > ADGAS DAS ISLAND UAE
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
>
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...