Dear Friends,
I would appreciate if you be able to give your advice to me about the designing of a very high pressure line heater.
I am in process to design a line heater with the following information:
MAWP: 10000 PSI @ -40/ 250 F
Corrosion Allowance: 1/16”
RTJ Weld Neck: 3+1/16” 10K API
4130 Material
I realize that this does not fall under the normal construction codes ( B31.3 ). However I am unfamiliar with what direction to take. Your help in this matter is greatly appreciated.
Sincerely yours’
Alia
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments