Do the Die- Penetrant test, or if possible RT, then clean the joint if not defect not found, then start the preheating till 200 F or  the last  left temperature, then start the weld, then clean and after cooling again do the die- Penetrant or RT,

 

Members may keep their views.

Bagesh.

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of carlosoliveros@terra.com
Sent: Friday, August 08, 2008 7:08 AM
To: materials-welding@googlegroups.com
Subject: [MW:1006] Interrupted welding with Pre-Heat & PWHT

 






----- Original Message -----
From: carlosoliveros@terra.com
To: materials-welding@googlegroups.com
Cc:
Sent: Thu 07/08/08 16:31
Subject: Fwd: No Subject



How are alls, Excuse me, I have a question, if i have a weld, Material AP1 5L X-60(P1) 42" SCH 1,25"  Pre heat 200 F, Process GTAW/SMAW, First pass GTAW 3/32" and then shall interrupted because raining or other cass what is the recomendation?

 

Regards



</HTML


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...