[MW:1006] Interrupted welding with Pre-Heat & PWHT






----- Original Message -----
From: carlosoliveros@terra.com
To: materials-welding@googlegroups.com
Cc:
Sent: Thu 07/08/08 16:31
Subject: Fwd: No Subject


How are alls, Excuse me, I have a question, if i have a weld, Material AP1 5L X-60(P1) 42" SCH 1,25"  Pre heat 200 F, Process GTAW/SMAW, First pass GTAW 3/32" and then shall interrupted because raining or other cass what is the recomendation?

 

Regards



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...