Dear Mr. Subramanium,

Please note that RT or any NDT cannot replace Hydro or Pneumatic test.
It can only certify the welded joint, not the whole pipe line.

R. Bose

On Jun 16, 10:21 am, "shiva.subramanium" <shiva.subraman...@wsiko.com>
wrote:
> Dear Members, Mr. Surya and Mr. Raghuram
>
> Due to water problem, you cannot go for pneumatic test based on TP = 110% of
> DP) because the hazard of energy release.
>
> Just calculate the pneumatic pressure for the system
>
> Hydrotest = 60 KG/cm2, so design pressure is around 40 Kg/cm2
>
> For pneumatic test, pressure shall be around 44 kg/cm2.
>
> Imagine the hazard of energy release with reference to the
> attachment(attached previous message of Criticality of Hydrotest pressure vs
> pneumatic pressure)
>
> So, better you can go for 100% RT/UT for all Butt joints and PT/MPT for
> attachment weld as per B31.3 para 345.9.
>
> S. Siva Subramanian
> World Services Italia S.p.A., Kuwait Operations,
> P.O. Box : 28928 - Safat : 13151 - Kuwait.
> Tel : +965 3262945 / 3260338 / 3263987 / 3263691/92, Ext.\ 207
> Mobile - 00965 632 7395
> E-mail :  shiva.subraman...@wsiko.com
>
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
>
> [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
> (Mumbai - PIPING)
> Sent: Monday, June 16, 2008 10:44 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:867] pressure testing
>
> Assuming your design code is B31.3, refer para 345 for the creteria (TP
> is 110% of DP)
>
> Also refer earlier message posted in this group titled  "Criticality of
> Pneumatic pressure test vs Hydrostatic on piping system"
> we should always remember that is necessary to evaluate
> the design aspects of material selection for piping lines to be
> submitted to pneumatic test: in these cases ASME B 31.3 require that the
> materials be guaranteed against their brittleness at the ambient
> temperature during pneumatic test.
> Typical cases are the plants where the ambient temperature could reach
> even minus 50^C (e.g. some parts of Russia).
>
> -----Original Message-----
> From: gajjalla surya prakash [mailto:gajja...@gmail.com]
> Sent: Monday, June 16, 2008 12:32 PM
> To: materials-welding@googlegroups.com
> Subject: pressure testing
>
> dear members,
>
> we are doing hydrotest for the piping systems and now facing the
> problem of water scarcity ,and our customer praposes to perform the
> pneumatic test .
>
> for example hydrotest pressure is 60kg/cm2 what should be the
> pneumatic pressure . where can we get this information.
>
> surya prakash gajjalla.
>
>
>
>  Scanned_ (2).pdf
> 141KDownload- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...