[MW:858] 857] Diffusible H2 content and Hydrogen cracking study

Dear Mr.Ragu,

Thanks for warning me. I just forget that Codes & standards should not be
copied in any form.

Thanks once again.

Regards,

S.Mathusoothanan

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
(Mumbai - PIPING)
Sent: 12 June, 2008 8:01 AM
To: materials-welding@googlegroups.com
Subject: [MW:857] Diffusible H2 content and Hydrogen cracking study


Dear Mr Mathusoothanan

Apriciate your posting, but I have to approve this message without the
attchements, since it is agianst the rules of this group (and all
members are requested to not post any codes/standards as attachements
in the group)

Thanking you for your co operation!

-----Original Message-----
From: mathu.subramanian [mailto:mathu.subramanian@kharafinational.com]
Sent: Thursday, June 12, 2008 10:20 AM
To: materials-welding@googlegroups.com
Subject: 851] Diffusible H2 content and Hydrogen cracking study

Dear friend,

E6013 is not the compatible electrode to weld Cr-Mo steels and it is
normal
carbon steel electrode. In Cr-Mo steels so many grades are there. Gr.1,
Gr.11, Gr.22, Gr.5, Gr.9, Gr.91. Please refer attached ASME Specs for
Electrodes & Materials. According to grade of material welding
electrodes is
to be selected.

As said by Mr Raghuram, two different AWS classifications can not be
compared for
diffusible hydrogen level. Two hydrogen levels of same AWS
classification
should be selcted.

I think the material grade you have selected might be Grade 9.

Regards.

S.Mathusoothanan

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula
Raghuram
(Mumbai - PIPING)
Sent: 12 June, 2008 6:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:851] Diffusible H2 content and Hydrogen cracking study


What type of Cr-Mo steel it is?
What is the basis of selecting E6013 for Cr-Mo steel?
Why diffusion hydrogen level required for E6013, when it is not a low
hydrogen electrode?
One can't compare the stress value with two different AWS
classifications; instead you can study by taking two different batches
of E9015B9 electrodes with different diff H2 levels (not comparing with
E6013) and test it!

Members please share your thoughts

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of mech
Sent: Wednesday, June 11, 2008 7:49 PM
To: Materials & Welding
Subject: [MW:846] on preheating effect


dear sir
i am a welding engg student and doing project on hydrogen cracking
of cr-mo steel by using implant test method.
the following result were observed

electrode diff hydrogen
level critical stress

E6013 (ruttile type) 5
ml 456 mpa
E9015 B9
10.6ml 500 mpa
according to theory if hydrogen level increases critical cracking
stress will decreases but in my exp critical cracking stress is coming
more in low level of hydrogen

i would like to have your comment on this result

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...