[MW:840] welding consumable for Yellow brass ASTM B36 UNS C27200

Members are requested to put appropriate subject line while posting new querry

also give more details about your querry, for e.g, what is your product form (bar, plate, pipe etc.) which welding process you are intended to use etc.

for this type of material (Cu+Zn) Joining by soldering and brazing is excellent. Joining by oxyacetylene welding is good, while only fair by gas shielded welding. Rod, bar, and wire may be resistance flash butt-welded.


-----Original Message-----
From: materials-welding@googlegroups.com on behalf of Muhammed Ibrahim
Sent: Tue 10/06/2008 20:33
To: materials-welding@googlegroups.com
Subject: [MW:839] Re: Clarification on Heat treatment-Reg.

*I** want a welding consumable for Yellow brass ( ASTM B36 UNS C27200
)material. Anybody can help me?

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...