Friday, June 20, 2008

[MW:873] RE: 872] Welding Tolerance

Yes you can, refer fig 328.4.3 in ASME B31.3 and/or ASME B16.25 (Butt welding ends)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zameer Mohammed
Sent: Thursday, June 19, 2008 1:16 PM
To: materials-welding@googlegroups.com
Subject: [MW:872] Welding Tolerance

 

Dear Friends,

We want to weld a 24'' SS PIPE A358 GR 321, 6.53 mm THK, to a Fitting / Pipe with same size and specification but with a Thickness of 9.53mm and 12.70 mm.

Can we do the welding of these items? What is the accepted tolerance as per ASME B31.3? Where can I find these details in ASME B313.3?

Thank you,

Regards,



Sabir


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...