Basically Cr-Mo steels need Pre heating and post heating when ever there are breaks for lunch, tea , shift changes. Interpass temperature maintenance is a MUST . Therfore even in site , the whole weld zone shall be in an enclosed environment so that there are no wind effects . For that matter any welding in an open wind environment is not advised.
Regards,
Tagore
On Wed, Jun 11, 2008 at 8:15 PM, <Sudipto_Banerjee@fwuk.fwc.com> wrote:
Pls. let me know if there should be any potential concerns of a reactor
made of ASTM A 387 Gr 22 CL1 in SITE ASSEMBLY with regards to welding, site
heat treatments and others.
If there is, then pls. let me know what are the points to be taken care by
the vendor.
Thanking you.
Best Regards,
Sudipto Banerjee
Man. no. B 4512
Equipment Engg. Department
Office no. 0091-(0)44-6622 2947
Mobile 1 (official) : 0044- 0 7733287865
Mobile 2 (personal) : 0091-9930005960
=======================================================
Confidentiality Notice
This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.
=======================================================
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Friday, June 13, 2008
[MW:864] Re: Site welding & heat treatment for ASTM A 387 Gr 22 CL1
Best would be provide electrical heating pads for the joints so that the minimum preheat can be maintained during the entire welding cycle
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment