[MW:866] Re: API 5L Material poperties

for mechanical  properties ref: API 5L (2000) line pipe specifications,6.1 and 6.2

 

Babu.P.R

--- On Fri, 6/13/08, asmat ullah <aubajwa@gmail.com> wrote:

From: asmat ullah <aubajwa@gmail.com>
Subject: [MW:861] API 5L Material poperties
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Friday, June 13, 2008, 4:16 AM

Hi friend,  could any body let me know where i can find mechanical properties (other than tensile and yield strength) of API 5L A, B, X42, X52, X60.., .....material?  I am interested in properties like poisson ratio, modulus of elasticity (young's modulus)... etc..  please help  Best Regards, Asmat Ullah          
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...