Tuesday, June 10, 2008

[MW:839] Re: Clarification on Heat treatment-Reg.

I want a welding consumable for Yellow brass ( ASTM B36  UNS C27200 )material. Anybody can help me?
 
2008/6/10 Owen Jenkins <owen@osjl.co.uk>:
For the notes to go with it, go to http://www.hghouston.com/mtechart.html.
 
Regards,
Owen Jenkins.
----- Original Message -----
Sent: Monday, June 09, 2008 4:01 PM
Subject: [MW:836] Re: Clarification on Heat treatment-Reg.

attachement gives the basic knowledge on this in graphical way, good one

On Mon, Jun 9, 2008 at 6:55 PM, Prabhakar h <hb.prabhakar@gmail.com> wrote:
Dear Shabbir,
 
Thanks a lot for your prompt response and sorry even i cud not catch up quite a while as i was held up with my ASME Audits.
 
Your Explanation was usefull and it would be better if you cud tell us at what conditions we go for the HT and how the same is selected???
 
Prabhakar.H

 








--
Thanks & Regards
Muhammed Ibrahim PK
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---