Gentlemen, Is PWHT can be avoided if the welded head (2 piece construction) performs normalizing after forming ? Head MOC : SA516 Gr 70, 45 mm thk, fabricated by welding the blank in two pieces. Complete vessel not required PWHT. Thanks & Regards Muhammed Ibrahim PK -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmMorLP3zvhePLHgVGFbcpx-t-%2BSd3M6EQpsfpHrAs38Ow%40mail.gmail.com .
Materials selection, welding, forming, Heat treatment, corrossion, NDT