[MW:14009] Re: Speed of Tensile Test

Normally Steady & uniform Load application during the tensile test is necessary, the speed of the tensile test is not mandatory according to my knowledge but high rate of loading is avoided. On Mar 28, 4:39 pm, Pushpraj Anand < pushprajanan...@gmail.com > wrote: > What is the speed of tensile test for Procedure qualification as per section IX? > > i read some coads they recommended for some speed of tensile test,is > it mandatory to follow or we can do at any speed? > -- > Regards, > Pushpraj Anand -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

[MW:14006] Speed of Tensile Test

What is the speed of tensile test for Procedure qualification as per section IX? i read some coads they recommended for some speed of tensile test,is it mandatory to follow or we can do at any speed? -- Regards, Pushpraj Anand -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

[MW:14005] P-91 material and Welding

Dear Experts... Can anyone provide me PPT on P91 material and how to perform welding and what are the special precaution need to be taken..... rgds Rohit -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Re: [MW:14004] PWHT OF P91 BY INDUCTION HEATING

Temperature differeancr is lesssthan 20-30 degree is acceptable.  how you can measure inside and out side temperature.you put 3 thermocouple 120 degree aprat out dide of the pipe and the temerature differeane max is 30 dedegree On Sat, Mar 24, 2012 at 5:36 PM, sandeep monody < smv.monody@gmail.com > wrote: Dear experts,   In my site we conducted a demonstration of PWHT on SA335 P91 material (OD-450mm X 70mm Thk) as our clients requirement and details as given below.   Heating/cooilng rate;-60 deg C,Holding temparature:-760deg C and holding time:-180minutes,Heating band width:-210mm and insulation band width 630mm,Heating method :-Induction heating   During pwht we observed a temparature difference on outside and inside of pipe more than 80 deg C.   Now problem is that client is not accepting this method and asking for uniform temparature in outside and inside of pipe.   How can i control temparature at both sides? Is it possible a uniform temp on both side with in...

Re: [MW:14003] PWHT OF P91 BY INDUCTION HEATING

Dear Pradip Sir, Thank you very much for your valuable information. Still some doubts are there as given below. As per AWS D10.10( Clause2.3.1)temperature variation up to 83deg is acceptable and AWS D10.10 itself says that there is no way to eliminate temperature variation though out the wall thickness(Clause 2.3). Actually in our site we have materials with various thicknesses and some up to 139mm and now question is.. what will be the temperature variation for 139mm thickness(On jobs its not possible to measure inside temperature). Have any equation or formula to find out the temperature variation throughout the thickness? Have any role of Thermal conductivity of P91 in this case? Is it possible a uniform temperature at OD and ID regardless of thickness? Awaits for your reply Thanks and regards Sandeep QC Engineer -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For ...

Re: [MW:14002] B31.3 PWHT requirement P1 materials

Hi mauricio,   Yes PWHT is required in this case.   Thanks Ravish On Tuesday, December 20, 2011 9:06:31 AM UTC+5:30, Raghuram Bathula wrote: Yes it is required for Thickness > 0.75" (20mm) On Tue, Dec 20, 2011 at 4:43 AM, mauricio padilla < mauricio_padilla_f@yahoo.com > wrote: Dear,   Please I need your Help, about ASME B31,3.   I need to know if it is required PWHT.   CASE:   Pipe A106 Grb (PN 1) wall thickness  0.844"   B31.3   Chapter V   Table 331.1.1   According to table 331.1.1 really is it necessay PWHT.   Please tell me   Is it correct?.   Best regards   Mauricio     -- To post to this group, send email to materials-welding@ googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@ googlegroups.com For more options, visit this group's bolg at http://materials-welding. blogspot.com/ The views expressed/exchnaged in...

[MW:14001] ASTM A182 F22 CL3 OVER stellite-6 welding criticality.

Dear experts, we are doing stellite welding in PTAW PROCESS.The base material ASTM A182 F22 CL3 in that over we are doing ST-6 HARDFACING.we are doing two layers .Each layer deposit height is 2.5mm.After PWHT & PROOF MACHINING deposit height is 4mm each side in proof machining we are doing LPI means it is 100 % defect free.BUT after final machining deposit height is 3mm.in that we are found lot of LPI ROUNDED INDICATIONS.So all the components are IN FIANLLY REJECTED.Please give the solution ASAP. REGARD'S M.VENKATESAN Q.C.ENGINEER OMPLASSYSTEMS. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicab...